Conoco ANDEROL® PQ AA 1000 White Mineral Food Grade Gear Oil, ISO Grade 1000, SAE Gear Oil Grade 1000
Subcategory: Fluid; Lubricant
Close Analogs: Anderol® is a registered trademark of The Anderol Company.
Material Notes: Description: ANDEROL PQ AA Series Gear Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Gear Oils provide excellent lubrication protection for gear sets, bearings, pumps and chain applications. The heavier viscosity grades can be used in worm gear applications with no harm to yellow metals. PQ food grade lubricants are approved, recommended and field tested by many OEMs in the food processing, baking, bottling, canning, meat processing and pharmaceutical industries. PQ food grade lubricants are listed by NSF International under “USDA Regulations, Proprietary Substances and Nonfood Compounds.” Information provided by ConocoPhillips.
| Available Properties |
- Specific Gravity
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Four Ball Extreme Pressure, Weld Load
- Four Ball Wear
- Pour Point
- Flash Point
- Copper Corrosion
- Rust Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|