DuPont Krytox® 101 GPL Oil
Subcategory: Fluid; Perfluoropolyether (PFPE)
Close Analogs: Information provided by DuPont Performance Lubricants.
Material Notes: Krytox® GPL 100–107 oils are clear, colorless, fluorinated synthetic oils that are nonreactive, nonflammable, safe in chemical and oxygen service, and are long-lasting. Krytox® is a perfluoropolyether (PFPE)—also called perfluoro-alkylether (PFAE) or perfluoropolyalkylether (PFPAE). The polymer chain is completely saturated and contains only carbon, oxygen, and fluorine. On a weight basis, a typical Krytox® oil contains 21.6% carbon, 9.4% oxygen, and 69.0% fluorine.
| Available Properties |
- Density
- Kinematic Viscosity at Room Temperature
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Evaporation Loss
- Coefficient of Friction
- Four Ball Wear
- Falex Load Test
- Oil Separation
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Pour Point
- ISO Grade of Oil
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|