Enviro Tech International EnSolv® Ionic n-Propyl Bromide Vapor Degreasing Solvent
Subcategory: Fluid
Close Analogs: Information provided by Enviro Tech International.
Material Notes: EnSolv-Ionic is the perfect direct replacement for TCE, Perchloroethylene, 1,1,1-Trichloroethane, HCFC-141b, Freon and other hazardous or discontinued vapor degreasing, ultrasonic and manual cleaning solvents. EnSolv-Ionic was developed to not only remove rosin flux, no-clean flux, oil, grease and wax contaminants, but also to remove residual halide salts, ions and other polar contaminants that often result in component failures. EnSolv-Ionic is a patented azeotropic mixture that can be distilled and reused through numerous cycles before it needs to be replaced. EnSolv-Ionic is compatible with all metals and many plastics and other materials typically cleaned in vapor degreasers or by other methods.
| Available Properties |
- Specific Gravity
- Water Absorption
- Vapor Pressure
- Dielectric Breakdown
- Specific Heat Capacity
- Boiling Point
- Flammability Test
- Acid Acceptance, as NaOH
- Acidity , as HCl
- Appearance
- Base Materials Meets ASTM D6368
- Evaporation Rate (Butyl Acetate = 1)
- Flash Point TCC
- Kauri Butanol Number
- Vapor Density (air = 1)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|