ExxonMobil Mobil 1 Gear Lubricant LS 75W-140
Subcategory: Fluid
Material Notes: Mobil 1 Synthetic Gear Lubricant LS 75W-140 is a supreme performance, synthetic, multi-purpose, automotive gear lubricant designed to meet the highest level performance requirements of many modern passenger vehicles in all types of operating conditions including limited slip applications, as well as deliver outstanding power transfer performance. Compared to conventional hypoid gear lubricants, Mobil 1 Synthetic Gear Lubricant LS 75W-140 performs exceptionally over a wide range of temperatures. Mobil 1 Synthetic Gear Lubricant LS 75W-140 achieves this through a unique proprietary combination of synthetic baseoils and a unique additive system including the SuperSyn antiwear system., that deliver optimized viscosity-temperature properties together with the highest level of inherent formulation stability and protects against thermal and oxidative degradation, wear and corrosion, viscosity loss associated with premature shearing. Mobil 1 Synthetic Gear Lubricant LS 75W-140 meets the API Service GL-5 EP gear oil service classification.Mobil 1 Synthetic Gear Lubricant LS 75W-140 is recommended for use in modern high performance vehicles like sport utility vehicles , vans and light duty trucks requiring API GL-5 performance that require excellent durability; Mobil 1 Synthetic Gear Lubricant LS 75W-140 is intended for initial fill, topping-off or refilling differentials, final drives, transfer cases and other gear applications where lubricants meeting API Service GL-5 and multi-purpose or mild EP gear lubricants are recommended; Mobil 1 Synthetic Gear Lubricant LS 75W-140 can also be used in rear axles where API Service GL-4 lubricant is recommended; Not recommended for automatic, manual or semiautomatic transmissions for which engine oil or automatic transmission fluids are recommended; Recommended for many limited slip applications. For certain high level LS applications, additional limited slip additive may be required if axle chatter is observed.
| Available Properties |
- Density
- Viscosity Measurement
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Pour Point
- Flash Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|