ExxonMobil Mobilfluid LT 75W-80
Subcategory: Fluid
Material Notes: Mobilfluid LT is an extra high performance multipurpose tractor lubricant engineered to meet or exceed tractor transmission, drivetrain, and hydraulic fluid requirements. This product is designed to optimize the performance of agricultural and industrial tractors operating in a wide range of environments and especially in low ambient temperature applications. This next generation product combines select base oils and an advanced additive package to deliver a variety of lubricant performance properties required by various applications.Heavy-duty transmissions, differentials, final drives, hydraulic systems, power steering systems, wet brakes, PTOs, and hydrostatic drives used in agricultural, contractor, and industrial applications; Recommended for top-up and refill of systems; Suitable for transmission applications requiring Type A (Suffix A), Dexron, and Type F fluids; Recommended for hydraulic and transmission systems where an SAE 10W-20 engine oil is specified; Do not use in passenger car automatic transmissions
| Available Properties |
- Density
- Brookfield Viscosity
- Viscosity Measurement
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Pour Point
- Flash Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|