ExxonMobil Mobil Vactra Oil Numbered Series 1

 

Subcategory: Fluid

Material Notes:
The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They are formulated from high-quality base stocks and performance balanced with a progressive additive system that provides low frictional properties, excellent corrosion protection and foam resistance. A unique advanced additive package helps reduce stick-slip and chatter under thin film, boundary lubrication conditions. This allows smooth, uniform motion at design travel speeds. The Mobil Vactra Oil Numbered Series have been optimised to provide excellent separability from aqueous coolants in coolant systems while minimising the corrosive effects of high pH coolants on lubricated surfaces. The base stocks and additive package have been carefully selected to protect slides and ways while still providing good filterability. This is important because reduced flow or plugged applicator filters will increase stick-slip, chatter and wear. The metal-wetting and adhesive agents form uniform films that resist squeezing from way surfaces while the machine is not in operation.

Mobil Vactra Oil Numbered Series products are recommended both as slideway lubricants and as fluids for moderate service machine tool hydraulic systems. These oils are designed for use with all combinations of cast iron, steel and non-metallic way materials. Mobil Vactra Oil Numbered Series may be applied by hand, forced-feed lubricator or in flood application by circulation system. Their extreme pressure properties make them suitable for all types of gears found in machine tools. They should not be used in circulation systems where bulk oil temperatures exceed 66ºC. Mobil Vactra Oil No. 2 is recommended for horizontal slideways on small to medium size machine tools. It is also suitable for flood application in large machines; Mobil Vactra Oil No. 3 is recommended for dual-purpose gear and way lubrication systems; Mobil Vactra Oil No. 4 is the normal recommendation for large machines where way pressures are high or good precision is required. It is also recommended for vertical and inclined slideways where drain-down can be a problem; Mobil Vactra Oil Numbered Series can be used for lubrication of ballscrews, linear guides, headstocks, translating screws, spur and bevel gears, and lightly loaded worm gears; Applications where conventional mineral oil contamination of the aqueous coolants shortens coolant batch life

Available Properties
  • Specific Gravity
  • Viscosity Measurement
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Four Ball Extreme Pressure, Weld Load
  • Four Ball Wear
  • Pour Point
  • Flash Point
  • Copper Strip Corrosion
  • FZG 4-Square Load Support, DIN 51354, Fail Stage
  • Rust Prevention, Distilled Water
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。