ExxonMobil Mobil SHC PM Series 320

 

Subcategory: Fluid

Material Notes:
Mobil SHC PM Series products are supreme performance synthetic lubricants specifically designed for the most demanding industrial paper machine circulating systems. They are engineered to provide exceptional lubrication characteristics not attainable with conventional premium mineral oil-based fluids. The Mobil SHC PM Series oils are formulated to provide maximum protection of gears and bearings operating under the most severe conditions. They have very low pour points and a naturally high viscosity index (VI) which helps ensure good low temperature start-up while maintaining excellent viscosity characteristics at very high temperatures. The fluids are very shear stable and maintain viscosity control even when subjected to severe mechanical shear in heavily loaded bearings and gears. Their low traction coefficient and high viscosity index can help result in lower energy consumption and reduced component operating temperatures. Mobil SHC PM Series oils are formulated with synthesised hydrocarbon fluid (SHF) base oil technology and a proprietary additive system carefully balanced to attain high performance standards These fluids permit the use of higher steam pressures, temperatures and machine speeds common in high output paper machines and calendar rolls. Their outstanding hydrolytic stability and filterability assure excellent performance in the presence of water and the ability to retain effective filtration even at very fine filtration levels. They readily separate water and retain their colour characteristics for extended periods of operation under severe conditions.

Lubrication of severe industrial paper machine circulating systems; Application involving circulation systems operating over a wide temperature range such as calendar rolls; Systems that must be started and brought on line quickly; Circulation systems lubricating gears and bearings

Available Properties
  • Specific Gravity
  • Viscosity Measurement
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Total Acid Number
  • Pour Point
  • Flash Point
  • Copper Strip Corrosion
  • Demulsibility Time (min)
  • FZG 4-Square Load Support, DIN 51354, Fail Stage
  • Rust Prevention, Distilled Water
  • Rust Prevention, Synthetic Sea Water
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。