ExxonMobil Mobilmet S-122
Subcategory: Fluid
Material Notes: Mobilmet S-122 is a water-soluble, general-purpose cutting oil designed for moderate-duty cutting and metalworking operations. Mobilmet S-122 fluid is formulated with select base oils and fortified with soaps, sulfonates and coupling agents. It also contains stabilizers to control odor and provide long service life.Mobilmet S-122 is recommended for a wide range of machining operations on both ferrous and non-ferrous metals; Cutting and grinding operations requiring water-soluble fluids; Applications where enhanced cooling is desired; Machining and grinding operations on both ferrous and non-ferrous metals; Mobilmet S-122 is used where normal water hardness is 300 ppm
| Available Properties |
- Density
- Kinematic Viscosity at 40°C (104°F)
- Pour Point
- Flash Point
- Emulsion Test, MM 1387
- Freeze Test, MM 1388
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|