ExxonMobil Exxon Hyjet V
Subcategory: Fluid
Material Notes: Exxon HyJet V is a Type V fire-resistant phosphate ester hydraulic fluid, which is superior in thermal and hydrolytic stability to commercially available Type IV hydraulic fluids. Better stability means extent of fluid degradation in aircraft systems will be less than Type IV fluids, in-service fluid life will be longer, and aircraft operator maintenance costs will be lower. HyJet V provides excellent high and low temperature flow properties (kinematic viscosities) and rust protection. HyJet V has also demonstrated an improvement over the erosion protection performance afforded by Type IV fluids.Exxon HyJet V is designed for use in commercial aircraft phosphate ester hydraulic systems. It meets the SAE AS1241 requirements and is included in the Airbus NSA307110 and Boeing BMS 3-11M qualified products list. It is compatible in all proportions with commercial Type IV and Type V phosphate ester aviation hydraulic fluids.
| Available Properties |
- Density
- Specific Gravity
- Viscosity Measurement
- Viscosity Measure
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Evaporation Loss
- Total Acid Number
- Bulk Modulus
- Electrical Resistivity
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Pour Point
- Flammability Test
- Flash Point
- Foam Sequence I, ASTM D1136
- Foam Sequence II, ASTM D893
- Foam Sequence III, ASTM D893
- Particle Count, NAS 1638 Class
- Sonic Shear Stability, KV change %
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|