ExxonMobil Mobil Aero HFA

 

Subcategory: Fluid

Material Notes:
Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with excellent low temperature properties, good anti-wear performance, and good chemical stability. Mobil Aero HFA and HF are composed of mineral base oil stock and contain shear-stable VI improvers; Mobil Aero HFS is a synthetic polyalphaolefin-based fluid.

Mobil Aero HFA is a premium quality fluid that meets the requirements of the U.S. Military specification MIL-H-5606A (now obsolete). It has a very high VI and is suitable for use at temperatures down to -54 ºC (-65 ºF). While this quality fluid is no longer used by the U.S. Military, it is still used in some older, small private, and commercial aircraft. It is also used in industrial and commercial equipment requiring good fluidity at very low temperatures, where Mobil Aero HFA provides long, trouble-free service over a wide range of operating conditions. Mobil Aero HF is a premium quality fluid that is approved against the most current version of U.S. Military specification MIL-PRF-5606. It has physical properties very similar to Mobil Aero HFA, and also meets "super-clean" requirements required by modern aircraft hydraulic systems. It is intended primarily for military aircraft, but it is also used as a hydraulic fluid for small private and commercial aircraft, and as a strut fluid in landing gear of large commercial aircraft. It is a NATO Code Number H-515 fluid. Mobil Aero HFS is a synthetic polyalphaolefin lubricant that is approved against the most current version of U.S. Military specification MIL-PRF-83282. It does not contain a viscosity index (VI) improver. It is designed for use at temperatures down to -40ºC (-40ºF). It provides lower flammability and volatility and improved stability, but has a higher viscosity at low temperature then Mobil Aero HF. It meets the "super-clean" requirements. It is intended primarily for U.S. military aircraft.It is a NATO Code Number H-537 fluid.

Available Properties
  • Specific Gravity
  • API Gravity
  • Viscosity Measurement
  • Viscosity Measure
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Evaporation Loss
  • Total Acid Number
  • Bulk Modulus
  • Four Ball Wear
  • Pour Point
  • Flash Point
  • Color
  • Copper Strip Corrosion, ASTM D130
  • Foam Sequence I, ASTM D1138
  • Low Temperature Stability
  • Oxidation Corrosion Stability
  • Rubber Swell, %
  • Sonic Shear Stability, KV change %
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。