ExxonMobil Exxon Aviation Oil Elite 20W-50
Subcategory: Fluid
Material Notes: Aviation Oil Elite 20W-50 is a premium quality, semi-synthetic, ashless-dispersant aviation piston engine oil. It is formulated from select, highly refined mineral base oils, a polyalphaolefin synthetic base oil, and ashless performance additives providing outstanding engine cleanliness, wear protection, and corrosion protection. Aviation Oil Elite 20W-50 is designed to satisfy the requirements of all opposed piston engine manufacturer’s requirements under a wide range of climatic conditions.Exxon Aviation Oil Elite 20W-50 is U.S. Military approved under SAE J1899, which replaced MIL-L-22851D and is listed in the U.S. Military Qualified Products List QPL-1899. It is approved by and included in the Qualified Products Lists of Teledyne Continental, and Textron Lycoming and it is designed to satisfy the requirements of all opposed piston engine manufacturers. It provides an alternate means of compliance with FAA AD 80-04-03-R2 par.b.1. New or newly overhauled aircraft engines should be broken in according to the engine builder’s recommended procedure. Many engine manufacturers advise running in on straight mineral oils for the first 25 to 50 hours of operation. In all cases, however, the engine manufacturers recommendations should be followed, since the run in procedure can vary from engine to engine. Aviation Oil Elite is compatible with non-dispersant mineral oils as well as other ashless-dispersant oils that meet the requirements of MIL-L-22851D/SAE J1899. It can also be used in high-time engines that have previously used a straight mineral oil. In this case it is advisable to carry out the oil-screen inspection recommended by the engine manufacturer.
| Available Properties |
- Density
- API Gravity
- Viscosity
- Viscosity Measurement
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Ash
- Total Acid Number
- Pour Point
- Flash Point
- Copper Strip Corrosion, ASTM D130
- Foam Sequence I, ASTM D1141
- Foam Sequence II, ASTM D893
- Foam Sequence III, ASTM D893
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|