ExxonMobil Mobil Polyrex EM

 

Subcategory: Fluid

Key Words: NLGI Grade 2

Material Notes:
Super-premium Mobil Polyrex EM Series grease is specially formulated for electric-motor bearings. The advanced thickener formulation and proprietary manufacturing techniques provide improved bearing performance and protection for long electric motor life.

Mobil Polyrex EM greases are recommended by many major bearing and electric motor manufacturers for long-life lubrication of electric motor ball and roller bearings. Mobil Polyrex EM 103 is more specifically recommended for applications such as vertically mounted bearings, or very large motors where a stiffer grease consistency may be required by the OEM, and low noise properties are not required. Mobil Polyrex EM greases have been shown to be compatible with a number of ExxonMobil lithium complex greases, as well as competitive electric motor mineral polyurea products, as determined by the methodology of ASTM D6185.  For specific questions about grease compatibility, contact your Mobil representative. Key applications include: Electric motor bearings; Fin fan bearings; High-temperature pump bearings; Factory-filled, sealed-for-life ball bearings; Ball or roller bearings operating at high temperatures where low oil separation is required; Polyrex EM for ball or roller bearings operating in noise sensitive environments

Available Properties
  • Viscosity Measurement
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Four Ball Wear
  • Penetration
  • Oil Separation
  • Dropping Point
  • Color
  • Copper Strip Corrosion, ASTM D4048
  • Corrosion Prevention, ASTM D1743
  • Grease Life, DIN 51821 (FE-9), hours
  • Low Temperature Torque, ASTM D1478, g-cm
  • Rust Prevention, Synthetic Sea Water
  • Water Washout, ASTM D1264, wt%
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。