Gwent Electronic Materials (GEM) Electrode Material: C2020628D1 Nickel Electrode Ink
Subcategory: Electronic/Magnetic Alloy; Ceramic/Metallic Coating
Material Notes: C2020628D1 Ink is an Nickel electrode ink designed for use with MLCC Tape. The ink contains 5% ceramic.C2020628D1 Ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use avoiding introduction of air bubbles. It is designed for printing on Ceramic tape. Information provided by Gwent Electronic Materials Ltd.
| Available Properties |
- Viscosity
- Storage Temperature
- Drying Temperature
- Dry Time
- Shelf Life
- BaTiO3 wt%
- Coverage cm2/g
- Fineness of Grind, microns
- Printing Mesh counts/inch
|
|
|
|