Gwent Electronic Materials (GEM) Termination Material: C2040929D12 Aluminum Ink
Subcategory: Electronic/Magnetic Alloy; Ceramic/Metallic Coating
Material Notes: Aluminum Ink is designed as a screen printing ink for termination of Barium Titanate based PTC devices. Particularly suited for PTC with low curie temperatures of 180°C.This Ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use avoiding introduction of air bubbles. Information provided by Gwent Electronic Materials Ltd.
| Available Properties |
- Solids Content
- Viscosity
- Storage Temperature
- Drying Temperature
- Dry Time
- Shelf Life
- Fineness of Grind, microns
- Printing Mesh counts/inch
|
|
|
|