Gwent Electronic Materials (GEM) Termination Material: C2020416D7 Copper Ink
Subcategory: Electronic/Magnetic Alloy; Ceramic/Metallic Coating
Material Notes: C2020416D7 is designed for BME End Terminations. The ink is designed for application using a Palomer dipping system. It can be used for Chipstar dippers, but the rheology needs of the customer have to be defined. It has excellent cosmetics and fires to a dense, smooth termination with high bond strength. It is designed to be used with standard Nickel/Tin Plating Systems.This Ink has been made at a ready to use viscosity and should be gently stirred before use avoiding introduction of air bubbles. Information provided by Gwent Electronic Materials Ltd.
| Available Properties |
- Density
- Solids Content
- Viscosity
- Brookfield Viscosity
- Storage Temperature
- Drying Temperature
- Dry Time
- Cosmetics
- Plateability
- Solderability
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|