Gwent Electronic Materials (GEM) 2 Part Silver Epoxy Adhesive: C1990419D2 Part 2 - Resin
Subcategory: Additive/Filler for Polymer; Adhesives, Sealants, and Coatings
Material Notes: The two components mixed together form a high conductive, strong adhesive layer. Can be used for screen-printing or other application methods.The two components C1990419D1 and C1990419D2 are both supplied at the correct viscosity ready for mixing. The 1:2 mixture should be stirred together gently to avoid introduction of air bubbles. Suitable for screen printing. Information provided by Gwent Electronic Materials Ltd.
| Available Properties |
- Viscosity
- Storage Temperature
- Volume Resistivity
- Processing Temperature
- Shelf Life
- Coverage cm2/g
- Fineness of Grind, microns
|
|
|
|