Gwent Electronic Materials (GEM) Electro Luminescent Display: C2040902D6 Carbon Ink for Electro Luminescent Lamps
Subcategory: Additive/Filler for Polymer; Adhesives, Sealants, and Coatings
Material Notes: This product is based on a unique curing process that results in the low temperature formation of a thermosetting polymer. This ink has excellent adhesion, chemical and environmental resistance properties. Although originally designed as a Back Electrode, the excellent conductivity of this ink makes it suitable as a replacement for Silver Ink in smaller EL Lamps.This Ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use to ensure complete homogeneity. Information provided by Gwent Electronic Materials Ltd.
| Available Properties |
- Viscosity
- Thickness
- Surface Resistivity per Square
- Cure Time
- Shelf Life
- Printing Mesh counts/inch
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|