Gwent Electronic Materials (GEM) Polymer Based Dielectric Material: D2040917D2 Polymer Dielectric
Subcategory: Additive/Filler for Polymer; Adhesives, Sealants, and Coatings
Material Notes: This material is a grey colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode. The formulation is designed for maximum flexibility. This product offers limited resistance to aggressive solvent attack.The paste is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The paste should be gently stirred before use avoiding introduction of air bubbles. It is a Polymer System for printing on polyester, PVC, Polycarbonate etc and on alumina. Information provided by Gwent Electronic Materials Ltd.
| Available Properties |
- Solids Content
- Viscosity
- Storage Temperature
- Dry Time
- Shelf Life
- Coverage cm2/g
- Printing Mesh counts/inch
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|