Gwent Electronic Materials (GEM) Polymer Based Dielectric Material: D2000222D2 Polymer Dielectric
Subcategory: Additive/Filler for Polymer; Adhesives, Sealants, and Coatings
Material Notes: This material is a blue colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode. The formulation is designed for maximum flexibility. This product offers limited resistance to aggressive solvent attack. This is part of a family of Polymer Dielectric Pastes designed for the protecting and defining of electrodes.The paste is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The paste should be gently stirred before use avoiding introduction of air bubbles. It is a Polymer System for printing on polyester, PVC, Polycarbonate etc and on alumina. Information provided by Gwent Electronic Materials Ltd.
| Available Properties |
- Solids Content
- Viscosity
- Storage Temperature
- Drying Temperature
- Dry Time
- Shelf Life
- Coverage cm2/g
- Printing Mesh counts/inch
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|