Gwent Electronic Materials (GEM) Carbon Based Working Electrode Paste: C2030519D4 Carbon/Graphite Ink
Subcategory: Ceramic/Metallic Coating; Adhesives, Sealants, and Coatings
Material Notes: Carbon Graphite Ink C2030519D4 is designed to be used for screen printing working electrodes. This is a carbon graphite ink which has been optimized to give superior electrochemical performance with good reversibility when using cyclic voltammetry. For optimum print properties and fine lines we would recommend the use of Carbon/Graphite C2000802D2.The ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use avoiding introduction of air bubbles. It is a Polymer System for printing on polyester, PVC, Polycarbonate etc and on alumina. Information provided by Gwent Electronic Materials Ltd.
| Available Properties |
- Viscosity
- Thickness
- Storage Temperature
- Surface Resistivity per Square
- Dry Time
- Shelf Life
- Coverage cm2/g
- Printing Mesh counts/inch
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|