Gwent Electronic Materials (GEM) Metallic Based Working Electrode Paste: C2041206D2 Gold Polymer Electrode Paste
Subcategory: Ceramic/Metallic Coating; Adhesives, Sealants, and Coatings
Material Notes: Gold Paste C2041206D2 is a screen printable gold polymer paste designed as a working electrode in electrochemical Biosensors. This paste is used as a working electrode in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries, in conjunction with counter and reference electrodes.The ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use avoiding introduction of air bubbles. It is a Polymer System for printing on polyester, PVC, Polycarbonate etc and on alumina. Information provided by Gwent Electronic Materials Ltd.
| Available Properties |
- Solids Content
- Viscosity
- Thickness
- Storage Temperature
- Surface Resistivity per Square
- Drying Temperature
- Dry Time
- Shelf Life
- Coverage cm2/g
- Fineness of Grind, microns
- Printing Mesh counts/inch
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|