Gwent Electronic Materials (GEM) Metallic Based Working Electrode Paste: C2000511D1 Platinized Carbon Ink
Subcategory: Ceramic/Metallic Coating; Adhesives, Sealants, and Coatings
Material Notes: Platonized Carbon Ink C2000511D1 is designed to be used for screen printing working electrodes. This product is a Platonized carbon graphite ink which has been optimized to give superior electrochemical performance. This product is particularly suited for use with Oxidized Enzymes where Hydrogen Peroxide is generated and detected.The ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use avoiding introduction of air bubbles. It is a Polymer System for printing on polyester, PVC, Polycarbonate etc and on alumina. Information provided by Gwent Electronic Materials Ltd.
| Available Properties |
- Viscosity
- Thickness
- Storage Temperature
- Surface Resistivity per Square
- Dry Time
- Shelf Life
- Coverage cm2/g
- Printing Mesh counts/inch
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|