Gwent Electronic Materials (GEM) LTCC Tape Product: C2000904D1 Platinum Ink
Subcategory: Ceramic/Metallic Coating; Adhesives, Sealants, and Coatings
Material Notes: Platinum Ink C2000904D1 is an ink formulated for screen printing onto LTCC tape. It is compatible with most LTCC tape systems on the market.The ink has been made at a ready to use viscosity and should be thoroughly stirred before use avoiding introduction of air bubbles. It can be printed on automatic and semi automatic screen printers. Information provided by Gwent Electronic Materials Ltd.
| Available Properties |
- Solids Content
- Viscosity
- Storage Temperature
- Surface Resistivity per Square
- Drying Temperature
- Dry Time
- Shelf Life
- Coverage cm2/g
- Fineness of Grind, max, microns
- Printing Mesh counts/inch
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|