Gwent Electronic Materials (GEM) Backlight Automotive Product: C2000808D1 Silver Backlight Ink

 

Subcategory: Ceramic/Metallic Coating; Adhesives, Sealants, and Coatings

Material Notes:
Silver Ink C2000808D1 is a low resistance ink designed for use as the heating bars and tracks on automobile backlights and other circuits on glass. It has a dark back color when printed and fired on float side of glass and is fully blendable with high resistance ink C2000808D2. It can be printed onto IR or UV black enamels.

Silver Ink C2000808D1 is a grey ink with a pine smell at a ready to use viscosity suitable for firing on glass to form conductive tracks. The ink should be gently stirred before use avoiding the introduction of air bubbles.

Information provided by Gwent Electronic Materials Ltd.

Available Properties
  • Solids Content
  • Viscosity
  • Storage Temperature
  • Surface Resistivity per Square
  • Drying Temperature
  • Dry Time
  • Shelf Life
  • Coverage cm2/g
  • Fineness of Grind, max, microns
  • Printing Mesh counts/inch
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。