Gwent Electronic Materials (GEM) Precious Metal Electrode Material: C2020411D1 Electrode Ink
Subcategory: Ceramic/Metallic Coating; Adhesives, Sealants, and Coatings
Material Notes: Electrode Ink C2020411D1 is a Silver Palladium (70/30) electrode ink, designed for use with Solufill Tape. It has been specifically formulated for use with PZT ceramics.The ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use avoiding introduction of air bubbles. It is designed for printing on Solufill tape. Information provided by Gwent Electronic Materials Ltd.
| Available Properties |
- Solids Content
- Viscosity
- Storage Temperature
- Dry Time
- Shelf Life
- Coverage cm2/g
- Fineness of Grind, microns
- Printing Mesh counts/inch
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|