Gwent Electronic Materials (GEM) Precious Metal Termination Material: C2040707D5 Silver Ink
Subcategory: Ceramic/Metallic Coating; Adhesives, Sealants, and Coatings
Material Notes: Silver Ink C2040707D5 is a lead free silver termination for use on electroceramics. Primarily designed for use on PZT, it can be used as lead free termination on other ceramics.The ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use avoiding introduction of air bubbles. Information provided by Gwent Electronic Materials Ltd.
| Available Properties |
- Solids Content
- Viscosity
- Storage Temperature
- Drying Temperature
- Dry Time
- Shelf Life
- Fineness of Grind, max, microns
- Fineness of Grind, microns
- Printing Mesh counts/inch
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|