Heatbath/Park Thermo-Quench Oil
Subcategory: Fluid
Material Notes: A "hot" or "marquenching" oil offering excellent thermal stability, high flash point and fast quenching rate. Information provided by Heatbath Corporation - Park Metallurgical.
| Available Properties |
- Saybolt Viscosity at 100°F
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
|
|
|
|
| Property Data |