Heatbath/Park Parquench 90 Water-Based Quenchant
Subcategory: Fluid
Material Notes: The higher molecular weight polymer package. It is generally used for higher alloy steels and all types of metals where the control of distortion is of prime importance. Typical concentration is 15%. Information provided by Heatbath Corporation - Park Metallurgical.
| Available Properties |
- Saybolt Viscosity at 100°F
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |