Heatbath/Park Sta-Hard 17 High Speed Hardening Salt
Subcategory: Ceramic
Material Notes: A neutral salt for hardening, annealing, normalizing, or preheating high speed tools. It is non-decarburizing, making it suitable for heating alloy tool steels which require high hardening temperatures. Information provided by Heatbath Corporation - Park Metallurgical.
| Available Properties |
- Melting Point
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |