Heatbath/Park #800 High Speed Hardening Salt
Subcategory: Ceramic
Material Notes: Working range covers temperatures frequently used in hardening and tempering steel. This product is also used as a high speed quench and draw. Information provided by Heatbath Corporation - Park Metallurgical.