Heatbath/Park #90 Casing High Speed Hardening Salt
Subcategory: Ceramic
Material Notes: An economical cyanide base salt which produces hard wear resistance properties for high speed tool steels in low dragout and/or low production use. It will maintain optimum operating characteristics over long periods of time, and provide an active operating bath on short notice. Casing is achieved at lower temperatures when iron nitride is selectively formed as a thin case on the tool surface. Information provided by Heatbath Corporation - Park Metallurgical.
| Available Properties |
- Melting Point
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |