Heatbath/Park Pen Kase 5 Carburizer
Subcategory: Fluid
Material Notes: Cyanide Liquid Carburizer. Water-soluble liquid carburizing salt offering easy cleaning, good fluidity and high stability. Will produce carbonitrided cases in lower temperature ranges and carbon cases in higher temperature ranges, usually up to about 0.050 inches. Information provided by Heatbath Corporation - Park Metallurgical.
| Available Properties |
- Melting Point
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|