Heatbath/Park Nu-Sal Steel Brazing Neutral Salt
Subcategory: Ceramic
Material Notes: The most economical salt for brazing performed within its working range. Silver and brass brazing are commonly done in Nu-Sal. It is non-hygroscopic and relatively non-corrosive to metal and fixtures. Information provided by Heatbath Corporation - Park Metallurgical.
| Available Properties |
- Melting Point
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |