Heatbath/Park Petroleum Pitch Coke Neutral Pack
Subcategory: Carbon
Material Notes: A granular material widely used as a packing medium for high carbon chromium tool steels to prevent undesirable carburization or decarburization. Used similarly to crushed coke but offers more uniform sizing and quality. "Blanking" is not usually required as it is for crushed coke. Information provided by Heatbath Corporation - Park Metallurgical.
| Available Properties |
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |