Heatbath/Park Parcure 275 Rubber Cure Salt
Subcategory: Ceramic
Material Notes: Nitrate/Nitrite Salt. An eutectic mixture offering the lowest possible melting point and the widest working range. (275 Parkettes) Information provided by Heatbath Corporation - Park Metallurgical.
| Available Properties |
- Melting Point
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |