Heatbath/Park Parcure 300 Rubber Cure Salt
Subcategory: Ceramic
Material Notes: A nitrite-free alternative for customers concerned with the introduction of nitrosamines from the alkali nitrite raw materials used in the production of commercial rubber cure salts. Within its working range, Parcure 300 exhibits viscosities less than or equal to more conventional salts now used; so resultant dragout could be less. Information provided by Heatbath Corporation - Park Metallurgical.
| Available Properties |
- Melting Point
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |