Heatbath/Park Partherm 430 Heat Transfer Salt
Subcategory: Ceramic
Material Notes: A popular heat transfer salt for use in the higher temperature ranges. It is more inert to ferrous alloys than Partherm 290 or 350 and considerably lower in cost. Its heat capacity and thermal conductivity are at least as good. (430 Parkettes) Information provided by Heatbath Corporation - Park Metallurgical.
| Available Properties |
- Melting Point
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |