Heatbath/Park Scale Kleen 5 Descaling Salt
Subcategory: Ceramic
Material Notes: A highly alkaline and oxidizing salt bath mixture used for the non-electrolytic descaling of most ferrous alloys and conditioning of surface oxides for subsequent removal in dilute acid. Nickel, chromium, cobalt and other alloys are also successfully descaled in Scale Kleen 5. Information provided by Heatbath Corporation - Park Metallurgical.