Lubriplate® SYNAC 46 Diester-Based Synthetic Air Compressor Fluid
Subcategory: Fluid
Key Words: Part Number L0933-
Material Notes: These diester-based synthetic air compressor fluids are outstanding for applications where the fluid is subjected to high temperature and high stress conditions over extended drain intervals.Synac Series Fluids are available in Pails & Drums. Information provided by Lubriplate
| Available Properties |
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Pour Point
- Flammability Test
- Flash Point
- SAE No.
|
|
|
|