Lubriplate® AC-0 Petroleum-Based Air Compressor Fluid
Subcategory: Fluid
Key Words: Part Number L0704-
Material Notes: Formulated to reduce carbon & varnish buildup. They contain fluid zinc to effectively fight friction & wear thus reducing heat & foaming. Available in six ISO grades.AC Series Air Compressor Oils are available in Bottles, Jugs, Pails, 1/4 Drums & Drums. Information provided by Lubriplate
| Available Properties |
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Pour Point
- Flammability Test
- Flash Point
- SAE No.
|
|
|
|