Lubriplate® Turbine Oil 32 Petroleum-Based Air Compressor Fluid
Subcategory: Fluid
Key Words: Part Number L0942-
Material Notes: This high-performance, zinc-free fluid meets the requirements of most centrifugal air compressors. Provides excellent oxidation resistance. Turbine Oil 32 is available in Drums. Information provided by Lubriplate
| Available Properties |
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Pour Point
- Flammability Test
- Flash Point
- SAE No.
|
|
|
|