Lubriplate® G.S. X-Heavy Lithium Based Grease For Open Gearing
Subcategory: Fluid; Lubricant
Key Words: Part Number L0152
Material Notes: Lithium-based open gear grease made for all types of open gears. Available in 4 formulas for a variety of conditions and temperatures. Gear Shield Extra Heavy is for adverse conditions.Applications: Open gears, adverse conditions. Excellent for fifth wheel applications. Gear Shield X-Heavy is available in Aerosol, Caulk Type Cartridges, Cans, Pails, 1/4 Drums & Drums. Information provided by Lubriplate
| Available Properties |
- Saybolt Viscosity at 100°F
- Kinematic Viscosity at 40°C (104°F)
- Penetration P(0), 1/10 mm
- Penetration P(60), 1/10 mm
- Minimum Service Temperature, Air
- Dropping Point
- Antiwear (AW)/ Extreme Pressure (EP)
- NLGI Grade
- Rust/Oxidative Addtives
- Water Resistant
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|