Paratherm HE® - Heat Transfer Fluid
Material Notes: Description: Paratherm HE® is a high flash and fire point heat transfer fluid. Engineered for higher thermal and oxidative stability, it is efficient and cost effective. Its greater purity allows it to strongly resist degradation while holding thermal properties and maintaining efficiency. This provides for low mainetance and solid performance over an extended operating life. Non-toxic, the HE fluid is safe to use and easy to dispose. It can be safely combined with spent lubricating oils and recycled locally.Information provided by Paratherm Corporation.
| Available Properties |
- Specific Gravity
- Density
- Kinematic Viscosity at 40°C (104°F)
- Molecular Weight
- Vapor Pressure
- Dielectric Strength
- Heat of Vaporization
- CTE, linear 68°F
- Boiling Point
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Pour Point
- Flash Point
- Refractive Index
- API Gravity
- Appearance
- Autoignition
- Color
- Corrosivity
- Feedstock
- Fire point
- Heat of Combustion
- Odor
- Pumpability
- Sulfur Content
- Total Acid Number
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|