Texaco Canopus® 46

 

Subcategory: Fluid

Close Analogs: CPS Number: 220544; MSDS Number: 8649

Material Notes:
Texaco Canopus oils deliver value through:

  • High resistance to forming emulsions due to excellent water separating characteristics.
  • Long lubricant life provided by outstanding stability.
  • Good lubricant compatibility — Compatible with other mineral-based and polyalphaolefin lubricants.

Texaco Canopus oils are high quality, high viscosity index uncompounded oils with excellent water separating characteristics.

Texaco Canopus oils possess good natural thermal and oxidation stability. Their high viscosity index makes them suitable for use over a wide temperature range. In a circulating oil system, compressor, or lightly loaded gear case, they will maintain a high film strength, protecting metal parts. Lubricant-related deposits will be kept to a minimum due to the excellent stability of these oils. System contaminants such as dirt and moisture can be easily removed from these oils by proper filtration.

Texaco Canopus oils are recommended for use in many circulating oil systems, as cylinder lubricants in double-acting reciprocating compressors, and for the lubrication of both cylinders and running gears of single-acting compressors.

Because of their compatibility, Texaco Canopus oils are good for flushing lubricant systems as well.

Texaco Canopus 100 is also recommended for use as a hot quenching oil for steel.

Texaco Canopus oils can be used for hand oiling. Their high viscosity index makes them suitable for use over a wide temperature range.

Do not use Texaco Canopus 13, 19, or 68 in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Available Properties
  • API Gravity
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Pour Point
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。