Recommended in Atlas Copco, Sullair, Ingersoll-Rand and Quincy rotary screw air compressors. Texaco Cetus PAO products meet the requirements of German DIN 51506 VDL standard.Texaco Cetus PAO oils are synthetic compressor oils. They are based on polyalphaolefin technology.
They provide outstanding thermal and oxidation stability, high viscosity index, high flash point, low pour point, and excellent hydrolytic stability.
Texaco Cetus PAO oils protect against rust, oxidation, and foaming, and have good antiwear properties.
The natural thermal and oxidation stability of these lubricants, due to their high level of purity and refinement, has been further enhanced by their unique additive systems.
The high thermal and oxidation stability reduces the formation of oxidation byproducts and acidic materials which will eventually cause deposits and varnish.
They are able to withstand relatively high temperature operations for extended periods of time. They have very good demulsibility characteristics allowing quick release of moisture.
They minimize entrained air, which could otherwise result in reduced lubricant film thickness and potentially lead to pump cavitation.
They are compatible with most elastomeric seal materials that are used with mineral oil based compressor lubricants.
Texaco Cetus PAO oils are formulated to provide outstanding lubricating qualities for air compressors, especially portable and stationary rotary, vane, and screw compressors.
Texaco Cetus PAO oils are recommended for industrial bearings and gears that require a synthetic gear oil that does not contain extreme pressure additives.
Texaco Cetus PAO oils are designed for applications with wide operating temperature ranges. They are especially effective in high temperature applications where outstanding thermal and oxidative stability are required.
Do not use in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed.
Do not use in breathing air apparatus or medical equipment.
Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.