Havoline® Automatic Transmission Fluid MERCON®/DEXRON®-III

 

Subcategory: Fluid

Close Analogs: CPS Number: 221854; MSDS Number: 8654

Material Notes:
Havoline Automatic Transmission Fluid MERCON/DEXRON-III delivers value through:

  • Protection against the formation of lacquers, sludge, or other harmful deposits.
  • Exceptional stability provided by excellent base oil and extra oxidation inhibitors.
  • Quiet Performance, especially effective in reducing transmission "chatter".
  • Fast circulation during cold weather and excellent lubricating body when hot.

Havoline Automatic Transmission Fluid MERCON/DEXRON-III is the latest high performance, multipurpose, pwer transmission fluit approved under Mercon® and Dexron® specifications. It is developed for passenger car and light truck automatic transmissions.

It is manufactured from select Group II base oils and additives that provide oxidation and thermal stability, friction control, load-carrying ability, corrosion and wear protection. It prevents the accumulation of deposits and the formation of sludge, varnish, and foam.

Under the most severe operating conditions, Havoline Automatic Transmission Fluid MERCON/DEXRON-III:

  • Maintains friction control for smooth shift action
  • Is specially formulated to prevent shudder
  • Retains low temperature fluidity and high temperature stability for long operating periods.
  • Protects automatic transmission fluid coolers from corrosion.
  • Practically eliminates transmission overhauls due to sludge, corrosion, wear of clutches and bands, gears and bearings, leakage past seals, and loss of frictional properties.

Havoline Automatic Transmission Fluid MERCON/DEXRON-III is designed for use in General Motors Corporation transmissions that require a DEXRON-II, DEXRON-II or DEXRON-IIE fluid, and Ford Motor Company transmissions that require a MERCON fluid. It is also used as a light oil in compressors, pumps and hydraulic systems.

  • Always check your owners manual to determine the proper automatic transmission fluid for your transmission.
  • Ford transmissions manufactured after 1996 may require a MERCON V.
  • Chrysler transmissions manufactured after 1996 require either ATF+3® or ATF+4®3.

Havoline Automatic Transmission Fluid MERCON V meets or exceeds:

  • Manufacturers performance requirements
    • Ford MERCON
    • General Motors DEXRON-III
    • Allison C4
    • Caterpillar TO-2
    • Denison P-46 Piston Pump
    • Vickers Pump
    • Voith DIWA Transmissions
    • AF transmissions

    Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

    Available Properties
    • API Gravity
    • Brookfield Viscosity
    • Viscosity Measurement
    • Saybolt Viscosity at 100°F
    • Saybolt Viscosity at 210°F
    • Kinematic Viscosity at 40°C (104°F)
    • Kinematic Viscosity at 100°C (212°F)
    • Pour Point
    • Flash Point
    • Color
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。