Texaco Regal® AW 100

 

Subcategory: Fluid

Close Analogs: CPS Number: 220628; MSDS Number: 8782

Material Notes:
Texaco Regal AW oil delivers value through:

  • High Temperature stability provides long lubricant life and resistance to formation of sludge and varnish on bearings and gears.
  • Excellent wear protection provides long bearing life and protects gears from scuffing.
  • Excellent water separability provides benefits for circulating oil systems subject to severe water contamination
  • Effective foam inhibition — Reduces the amount of entrained air in the oil, minimizing the possibility of pump cavitation and also prevents surface foam.

Texaco Regal AW 100 is a circulating oil formulated from high quality base stocks and a carefully balanced, zinc-free additive package. This provides excellent protection against wear for long bearing and gear life. Texaco Regal AW 100 has superior water separability properties and rust protection to deal with the severe water contamination that frequently occurs in circulating oil systems. Its outstanding oxidation stability minimizes deposit formation and leads to long lubricant life.

Texaco Regal AW 100 is a circulating oil designed for the steel industry. It is formulated to meet the needs of circulation systems serving high speed rollers and plain bearings in no-twist finishing mills It is also recommended for the lubrication of reduction gears and bearings where zinc-free oils are desired.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Available Properties
  • API Gravity
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Pour Point
  • Flash Point
  • FZG Pass Stage
  • Rust Prevention
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。