Texaco Spindura® 10
Subcategory: Fluid
Close Analogs: CPS Number: 220824; MSDS Number: 8371
Material Notes: Texaco Spindura oils deliver value through:- High oxidation stability — Longer service life than with conventional lubricants.
- Rust and corrosion protection — Gives excellent protection against corrosion of both copper and steel.
- Foam inhibition — Contains special foam suppressant. Eliminates both foaming and aeration problems.
- Excellent antiwear properties — Maximizes spindle life by controlling wear.
- Fast water separation — Minimize rust problems by fast release of water.
Texaco Spindura oils are premium oils manufactured especially to meet the severe requirements of spindle lubrication. They provide excellent antiwear protection, oxidation and corrosion inhibition, as well as foam suppression. Texaco Spindura oils are designed for use: - In machine tool spindles
- Textile applications
Do not use in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed. Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.
| Available Properties |
- API Gravity
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Pour Point
- Flash Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|