Texaco Hot Punch Compound H
Subcategory: Fluid; Lubricant
Close Analogs: CPS Number: 221979; MSDS Number: 9020
Material Notes:
Texaco Hot Punch Compound H is a dark, semi-fluid calcium soap thickened grease designed for use as a die lubricant. It contains graphite and telc, which enhance its lubricity. Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. Notes: - Determined on mineral oil extracted by vacuum filtration.
| Available Properties |
- Solids Content
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Penetration P(0), 1/10 mm
- Flash Point
- Color
- Texture
- Thickener, %
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|