Texaco Marfak® Multipurpose NLGI Grade 2
Subcategory: Fluid; Lubricant; Organic Soap Gellant
Close Analogs: CPS Number: 220958; MSDS Number: 8962
Material Notes: Texaco Marfak Multipurpose delivers value through:- Good water resistance — Provides lubrication in the presence of water.
- Good corrosion protection — Inhibited to protect gear and bearing surfaces.
- Good oxidation stability — Helps to ensure long life in storage and in use.
- Simplified lubrication — One grease designed to satisfy most general purpose, non-EP grease requirements.
Texaco Marfak Multipurpose is manufactured using selected, highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thickener, and rust and oxidation inhibitors. It is work stable and resists separation or throw out from antifriction bearings. It has a low oil bleeding tendency under pressure and is pumpable at low temperatures. Texaco Marfak Multipurpose satisfies general automotive and industrial applications that do not require the use of an EP grease. Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. Notes: - Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.
- Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.
- Determined on mineral oil extracted by vacuum filtration.
| Available Properties |
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Penetration P(60), 1/10 mm
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Pour Point
- Flash Point
- Dropping Point
- Color
- Corrosion, Copper Strip
- Texture
- Thickener, %
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|